Test Results On Woven Fabric
TEST SPECIMEN FLAME SPREAD RATE FUEL CONTRIBUTED FACTOR SMOKE DEVELOPED FACTOR
Asbestos Cement Board 0 0 0
Red Oak Flooring 100 100 100
Stratus (GRC) 10 15 0
Stratus (type "X" gypsum) 25 70 25
NOTE: The numerical flame spread rating and other test results referenced herein are not intended to reflect the hazards presented by this or any other material under actual fire conditions.

PERFORMANCE TEST

TEXTILE WALLCOVERING
STANDARD REQUIREMENTS

STRATUS RESULTS
ASTM D-1682
Tensile Strength (Grab)
50 lbs. minimum
50 lbs. minimum
Warp 190.3 lbs. Filling 210.0 lbs
ASTM D-2661
Tear Strength (Tongue)
6 lbs. minimum
6 lbs. minimum
Across Warp 38.7 lbs. Across Filling 19.8 lbs
ASTM D-4034
Resistance to yarn slippage of seams
25 lbs. minimum
25 lbs. minimum
Seam across warp 86 lbs. Seam across filling 85 lbs
ASTM D-2654 Procedure #2 Moisture Regain No published standard .05% excellent.
AATCC 8
Colorfastness to Crocking
Dry procedure Class 4 minimum
Wet procedure Class 3 minimum
Dry procedure Class 4.5 Wet procedure Class 4.5
AATCC 16A (Carbon Arc) Colorfastness to Light (Fadeometer) 40 Hours Class 4 minimum Class 5 (over 200 hours)